Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 9.50 MPa @Temperature 120 °C |
1380 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® HPN 9350 HS PA6 (Dry) Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res.. |