Flexural Strength 85.0 - 87.0 MPa
12300 - 12600 psi
ASTM D790M
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure at HOC +3
Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo..