Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 85.8 MPa | 12400 psi | ASTM D790 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Flexural Strength | 85.8 MPa | 12400 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY PCPBT 2525 PC/PBT Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |