Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 83.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 83.6 MPa
12100 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87180 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Flexural Strength 83.6 MPa
12100 psi
ASTM D790-03
Objet FullCure® 840 Vero Blue Resin for Rapid Prototyping
Information provided by American Precision Prototyping, LLC
Flexural Strength 83.6 MPa
12100 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne