Polymer Property : Flexural Strength = 82.76 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 82.76 MPa
12000 psi
ASTM D790
Lucent Polymers GPP-120 Polypropylene Homopolymer, 20% Glass Fiber Reinforced, Chemically Coupled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 82.76 MPa
12000 psi
ASTM D790
Lucent Polymers PBT-310 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Flexural Strength 82.76 MPa
12000 psi
ASTM D790
Lucent Polymers PBT-FR310 Polybutylene Terephthalate, Flame Resistant
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Flexural Strength 82.76 MPa
12000 psi
ASTM D790
Lucent Polymers PC/ABS-1003 Polycarbonate+ABS, Extrusion / General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.