Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 55.8 MPa | 8100 psi | |
Ohio Carbon Blank OCB EDM-200 Mechanical Grade Graphite Available in a range of sizes and shapes. |
|||
Flexural Strength | 55.8 MPa | 8100 psi | ASTM D790 |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Strength | 55.8 MPa | 8100 psi | ASTM D790 |
Chesterton ARC MXHT High temperature severe wear compound Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness o.. |
|||
Flexural Strength | 55.8 MPa | 8100 psi | |
3M Scotchkote™ CR 511 Epoxy Ceramic Surface Scotchkote Epoxy Ceramic CR 511 has been specifically developed as a 100% solids coating for resurfacing and lining to improve the efficiency of equipment in fluid flow environments.Product Features.. |
|||
Flexural Strength | 55.8 MPa | 8100 psi | |
BCC Products BC 7062-2H Epoxy Casting BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi.. |