Mechanical Properties Metric English Comments
Flexural Strength 8.96 MPa
1300 psi
ASTM D790
Techmer ES HiFill® TPU 1000
Availability: North AmericaForms: PelletsFeatures: High DensityAppearance: BlackInformation provided by TP Composites, Inc.
Flexural Strength 8.96 MPa
1300 psi
ASTM D790
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.