Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 51.6 MPa | 7480 psi | ASTM D790 |
I. Stern 745 Super High Impact Natural ABS Features:Super High ImpactExtrusionApplicationsPipeProfilesSheetInformation provided by I. Stern & Co. Inc. |