Mechanical Properties Metric English Comments
Flexural Strength 510 MPa
74000 psi
ASTM C1161
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite
High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co..