Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 510 MPa | 74000 psi | ASTM C1161 |
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |