Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 72.1 MPa | 10500 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87150 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |