Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 690 MPa | 100000 psi | ASTM D790 |
Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series. |