Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Glastic
Trade Name Laminates/Shapes
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 621 MPa
90100 psi
ASTM D638
Tensile Modulus 21.0 GPa
3050 ksi
ASTM D638
Flexural Strength 690 MPa
100000 psi
ASTM D790
Flexural Modulus 28.0 GPa
4060 ksi
ASTM D790
Compressive Strength 110 MPa
16000 psi
Transverse; ASTM D695
414 MPa
60000 psi
Axial; ASTM D695
Shear Strength 24.0 MPa
3480 psi
In-plane. ASTM D3914
Izod Impact, Notched 21.4 J/cm
40.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature 20.0 °C
5.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 200 °C
392 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Insulation Resistance, ASTM D257
Dielectric Constant 5.0

@Frequency 60 Hz
5.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 3.00 kV/mm
76.2 kV/in
1 in. axial in oil; ASTM D149
Arc Resistance 150 sec
150 sec
ASTM D495