Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | >= 470 MPa | >= 68200 psi | cold bending |
China-Yixing Longly Refractories Seggar SiC SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat.. |
|||
Flexural Strength | 470 MPa | 68200 psi | DIN EN 843-1 |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |