Mechanical Properties Metric English Comments
Flexural Strength >= 470 MPa
>= 68200 psi
cold bending
China-Yixing Longly Refractories Seggar SiC
SiC series products of SiC shelf boards, SiC pillars, SiC slab, SiC seggar kiln furniture, are formed using high-quality silicon carbide materials and high temperature binders by tons of high-vibrat..
Flexural Strength 470 MPa
68200 psi
DIN EN 843-1
CeramTec AT 79 Alumina, 99.6%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.