Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 41.0 - 46.0 MPa | 5950 - 6670 psi | ASTM D790M |
DSM Somos® 9120 Epoxy Photopolymer
(Unverified Data**) DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |
|||
Flexural Strength | 44.0 - 46.0 MPa | 6380 - 6670 psi | UV Postcure; ASTM D790M |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |