Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D-790 |
Plaskolite Optix® CA - 2000 HF-4-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D-790 |
Plaskolite Optix® CA - 2000 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D790 |
PolyOne LubriOne™ PC-000/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D790 |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D790 |
Ensinger Tecatron® XP-61L Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D790 |
Ensinger Tecatron® XP-82 Compression Molded PPS Compound, Filled with 15% PTFE and 30% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D790 |
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer.. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D-790 |
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D-790 |
Plaskolite West Optix® CA - 2000 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Flexural Strength | 66.2 MPa | 9600 psi | ASTM D790 |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance