Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 440 MPa | 63800 psi | ASTM D790 |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Flexural Strength | 440 MPa | 63800 psi | |
Lehmann & Voss LUVOCOM® 20-0951 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Flexural Strength | 440 MPa | 63800 psi | |
Lehmann & Voss LUVOCOM® 1/XCF/40 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Strength | 440 MPa | 63800 psi | DIN EN 843-1 |
CeramTec CD 110 Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati.. |
|||
Flexural Strength | 440 MPa | 63800 psi | ASTM-F394 |
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film Applications: thick films and lasers |