Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 60.5 MPa | 8770 psi | ASTM D790 |
BCC Products BC 8400 Urethane Casting BC8400 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8400 will exhibit high impact strength and yield thermoplastic-like parts. Some features i.. |