Polymer Property : Flexural Strength = 5201 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 35.86 MPa
5201 psi
ASTM D790
Lucent Polymers CPP-0307 Polypropylene, Mineral Filled, Impact Modified
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.