Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.86 MPa | 5201 psi | ASTM D790 |
Lucent Polymers CPP-0307 Polypropylene, Mineral Filled, Impact Modified Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |