Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.6 MPa | 5170 psi | ASTM D790 |
Multibase Multi-Flam™ 0102 Natural PP Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |