Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 346 MPa | 50200 psi | ISO 178 |
Solvay Specialty Polymers Kalix® 3950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3950 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Flexural Strength | 346 MPa | 50200 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |