Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 344 MPa | 49900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 344 MPa | 49900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON PX91060 PA 6 LNP* VERTON* PX91060 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added feature of this grade is: Structural. |
|||
Flexural Strength | 344 MPa | 49900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON PX91060 PA 6 (Asia Pacific) LNP* Verton* PX91060 is a compound based on Nylon 6 resin containing Long Glass Fiber. |