Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 496 MPa @Temperature 23.9 °C |
72000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati.. |
|||
Flexural Strength | 496 MPa | 71900 psi | ASTM D790 |
Quantum Composites HTC-9590 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9590 (127-51-3) is a 12K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristic.. |
|||
Flexural Strength | 496 MPa | 72000 psi | lengthwise; IPC TM-650 2.4.4 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |