Flexural Strength 3.30 MPa
479 psi
Multibase Multi-Flex® TPE A 8699 BLK
Multi-Flex® A 8699 is a TPE compound based on Kraton G polymer. It is used as medium density acoustic for noise abatement in the auto industry. Multi-Flex TPE contains Kraton™ G.Data provided by..