Material Notes:
Multi-Flex® A 8699 is a TPE compound based on Kraton G polymer. It is used as medium density acoustic for noise abatement in the auto industry. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955
Melt Flow 1.1 g/10 min
1.1 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
10 sec; ASTM D-2240
Tensile Strength, Ultimate 3.70 MPa
537 psi
ASTM D412
Elongation at Break 180 %
180 %
ASTM D412
Flexural Strength 3.30 MPa
479 psi
Flexural Modulus 0.0848 GPa
12.3 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 38.5 kN/m
220 pli
ASTM D624