Polymer Property : Flexural Strength = 46100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 318 MPa
46100 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6
LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing 50% Glass Fiber.
Flexural Strength 318 MPa
46100 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 (Asia Pacific)
LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber.
Flexural Strength 318 MPa
46100 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6
LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Strength 318 MPa
46100 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific)
LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Strength 318 MPa
46100 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66
LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Flexural Strength 318 MPa
46100 psi
ASTM D790
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent ..
Flexural Strength 318 MPa

@Temperature 22.8 °C
46100 psi

@Temperature 73.0 °F
ASTM D790
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..