Mechanical Properties Metric English Comments
Flexural Strength 258 MPa
37400 psi
ISO 178
Solvay TECHNYL® AR 218 V33 Black 34 N Nylon 66, 33% glass fiber, DRY
Description: Polyamide 66, reinforced with 33% of glass fiber, containing recycled material, for injection molding, specially stabilized to improve its resistance to automotive cooling liquids.Avail..
Flexural Strength 258 MPa
37400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RVL36 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RVL36 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE.
Flexural Strength 258 MPa
37400 psi
ISO 178
SABIC Innovative Plastics LNP Stat-kon OEL36A PPS
LNP* Stat-Kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This ..
Flexural Strength 258 MPa
37400 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED
LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Flexural Strength 258 MPa
37400 psi
ISO 178
SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear..
Flexural Strength 258 MPa
37400 psi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA
LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Flexural Strength 258 MPa
37400 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RVL36 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RVL36 is a compound based on Nylon 66 resin containing Long Glass Fiber, PTFE.