Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 230 MPa | 33300 psi | ASTM D790 |
Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled
(discontinued **) AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Flexural Strength | 230 MPa | 33300 psi | ASTM D790 |
Chase Plastics CP Pryme® NN130GMD2 (COND, 50% RH) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 230 MPa | 33300 psi | ASTM D790 |
Chase Plastics CP Pryme® NN130GMD2HS (COND, 50% RH) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated, Heat Stabilized Information provided by Chase Plastics. |