Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 230 MPa | 33400 psi | STN EN ISO 178 |
Plastcom SLOVAMID 6 GF 35 Polyamide 6, 35% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 35% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Flexural Strength | 230 MPa | 33400 psi | |
Plastcom SLOVAMID 66 GF 25 FRA 5 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, reinforced with 25% glass fibre and halogen flame retardant. Application in electrical industry: breakers, coilforms, covers, terminals. Slightly decreased flam.. |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
PolyOne OnForce™ LFT LF9200-5001 RS Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
PolyOne Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Flexural Strength | <= 230 MPa | <= 33400 psi | ISO 178 |
Polykemi AB SCANMID 6 B22^ E F40 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
Nilit FRIANYL A63 H-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 230 MPa | 33400 psi | |
Lehmann & Voss LUVOCOM® 1105-8416 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Flexural Strength | 230 MPa | 33400 psi | |
Lehmann & Voss LUVOCOM® 1-7882 Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Flexural Strength | 230 MPa @Strain 3.00 % |
33400 psi @Strain 3.00 % |
2 mm/min; ISO 178-A |
Lanxess Pocan® ECO T 3230 000000 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2mm/min; ASTM D790 |
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose) Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific) LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 (Europe-Africa-Middle East) Heat stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6 (Europe-Africa-Middle East) UV stabilized, 30% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC003SXS PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC003SXS is a compound based on PA 66 resin containing Carbon fiber. Added features include: Electrically Conductive, Heat Stabilized |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM-D790 |
Polyram Polytron P60B01 Homopolymer Polypropylene, Chemically Coupled 60% LGF A chemically coupled 60% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM-D790 |
Polyram Polytron P60B04 Homopolymer Polypropylene, Chemically Coupled 60% Long Glass Fiber A CHEMICALLY COUPLED PP 60% LONG GLASS FIBER WITH EXTRA LOAD OF ADDITIVES FOR DILUTION.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178-93 |
Wellman Wellamid® GF30-60 XE-WBK Nylon 6, 30% Glass Reinforced, Weatherable All information provided by Wellman Engineered Resins. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM C1161 |
M Cubed Technologies ASC-701 Aluminum alloy-70% SiC Metal Matrix Composite High stiffness, low density, low CTE composite. Components can be formed with complicated features, and can be machined to tight tolerances. Applications in high-precision equipment--semiconductor.. |
|||
Flexural Strength | 230 MPa | 33400 psi | cond; ISO 178 |
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45 45% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Flexural Strength | 230 MPa | 33400 psi | ISO 178 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Flexural Strength | 230 MPa | 33400 psi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 mm/min; ISO 178 |
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Strength | 230 MPa | 33400 psi | ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Flexural Strength | 230 MPa | 33400 psi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |