Polymer Property : Flexural Strength = 3250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 22.4 MPa
3250 psi
3M Scotchkote™ SG 527 Epoxy Metal Repair
Scotchkote Epoxy Metal Repair SG 527 is a specially packaged rapid curing synthetic metal repair compound for on site repairs to metal components such as leaking pipes, tanks, ducts, and radiators.P..