Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 22.4 MPa | 3250 psi | |
3M Scotchkote™ SG 527 Epoxy Metal Repair Scotchkote Epoxy Metal Repair SG 527 is a specially packaged rapid curing synthetic metal repair compound for on site repairs to metal components such as leaking pipes, tanks, ducts, and radiators.P.. |