Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 321 MPa | 46600 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Flexural Strength | 321 MPa | 46600 psi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Flexural Strength | 321 MPa | 46600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Europe-Africa-Middle East) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 321 MPa | 46600 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing 40% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Flexural Strength | 321 MPa | 46600 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF008H PPA (Asia Pacific) LNP THERMOCOMP* UF008H is a compound based on Polyphthalamide resin containing Glass Fiber. |