Polymer Property : Flexural Strength = 3000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Flexural Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v..
Flexural Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia..