Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1930 MPa | 280000 psi | |
CoorsTek ACI-Co6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Flexural Strength | 1930 MPa | 280000 psi | ASTM F417 |
CoorsTek Tungsten Carbide, WC Information provided by CoorsTek. |