Mechanical Properties Metric English Comments
Flexural Strength 188 MPa
27200 psi
ASTM D790
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil..