Flexural Strength 159 - 186 MPa
23000 - 27000 psi
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester
BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re..
Flexural Strength 165 - 186 MPa
24000 - 27000 psi
Bulk Molding Compounds BMC 810 General Purpose Molding Compound
BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is wel..