Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC 810 General Purpose Molding Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC 810 General Purpose Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 810 is a general purpose, very high strength compound suitable for compression, transfer and stuffer injection molding. It is characterized by excellent flow and controlled reactivity and is well suited for injection molding.Typical applications include structural components, mechanical applications, and bearing plates.
Physical Properties Metric English Comments
Specific Gravity 1.75 - 1.85 g/cc
1.75 - 1.85 g/cc
Water Absorption 0.15 - 0.25 %
0.15 - 0.25 %
24 hours, 23°C
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 52
45 - 52
Tensile Strength, Ultimate 68.9 - 82.7 MPa
10000 - 12000 psi
Elongation at Yield 2.0 - 2.5 %
2.0 - 2.5 %
Tensile
Flexural Strength 165 - 186 MPa
24000 - 27000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 131 - 152 MPa
19000 - 22000 psi
Izod Impact, Notched 7.47 - 9.08 J/cm
14.0 - 17.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 232 °C
>= 450 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Strength 16.7 kV/mm
425 kV/in
Short Time
Arc Resistance >= 180 sec
>= 180 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Mold Temperature 138 - 166 °C
280 - 330 °F