Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 129 - 157 MPa | 18700 - 22700 psi | |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |