Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1500 MPa | 218000 psi | |
China Tungsten NT3 Titanium Carbonitride Alloy Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high corrosion resistance to acids and alkalis and hi-tempe.. |
|||
Flexural Strength | 1500 MPa | 218000 psi | |
China Tungsten NT6 Titanium Carbide and Nitride Based Carbides Semi-finishing of low carbon steel, low alloy steel, gray cast iron, Si-AL alloy and finishing of stainless steel.Information provided by China Tungsten |
|||
Flexural Strength | >= 1500 MPa | >= 218000 psi | |
China Tungsten YGR7 Tungsten Carbide with Rare Earth Additive High hardness and strength, low friction, good wear resistance. Used as drawing dies for drawing and straightening of steels, non-ferrous metals and the alloy bars and tubings.Information provided b.. |
|||
Flexural Strength | 1500 MPa | 218000 psi | |
China Tungsten YT6S Tungsten Carbide Having the same wear resistance as YG6X but higher toughness. for tobacco cutters and rough and finish milling of cast iron.Information provided by China Tungsten |
|||
Flexural Strength | 1500 MPa | 218000 psi | |
China Tungsten YT772-2 Titanium Carbide and Nitride Based Carbides Good wear resistance and better toughness, relative impact resistance , for intermittent turning and milling of cast iron and steel parts.Information provided by China Tungsten |