Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 145.19 MPa | 21058 psi | ASTM D790 |
E-Polymers TEKAMID® HG20L 20% Glass Fiber Reinforced High Impact PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |