Flexural Strength 145.19 MPa
21058 psi
ASTM D790
E-Polymers TEKAMID® HG20L 20% Glass Fiber Reinforced High Impact PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..