Polymer Property : Flexural Strength = 2100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 2100 - 2600 MPa
305000 - 377000 psi
China Tungsten K510 Tungsten Carbide for Mining Purposes
High toughness and wear resistance, for pillar picks and coal cutting picksInformation provided by China Tungsten
Flexural Strength 2100 MPa
305000 psi
China Tungsten YG813 Tungsten Carbide
Optimum wear resistance, high bending strength and high resistance to bonding . Machining of refractory alloys, stainless steel and high manganese steel, etc.Information provided by China Tungsten
Flexural Strength 2100 - 2500 MPa
305000 - 363000 psi
China Tungsten Z20 Tungsten Carbide for Mining Purposes
Excellent wear resistance and toughness, for pillar bit drills.Information provided by China Tungsten