Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2.90 MPa | 421 psi | @ 20 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 2.90 MPa | 421 psi | @ 20 kg/m<sup>2</sup>; ASTM DC201 |
Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |