Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SF-400H Expandable Polystyrene (EPS) FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.03 - 1.05 g/cc
1.03 - 1.05 g/cc
Density 0.0149 g/cc
0.000538 lb/in³
Based on 70 times expansion
Bead Size 0.500 - 0.720 mm
0.0197 - 0.0283 in
JIS Z8801
Mechanical Properties Metric English Comments
Flexural Strength 2.90 MPa
421 psi
@ 20 kg/m<sup>2</sup>; ASTM DC201
Compressive Strength >= 1.20 MPa
>= 174 psi
@ 20 kg/m<sup>2</sup>; JIS A9511, ASTM D1621
Chemical Properties Metric English Comments
Blowing Agent Content 6.0 - 7.0 %
6.0 - 7.0 %
Pentane
Descriptive Properties Value Comments
Blocking <2%
Expandability 70 Times
Expansion for 5 min Cheil Method
Fusion >60%
Cheil Method
Polymer Content 93-94%