Polymer Property : Flexural Strength = 182.8 MPa
Polymer Property :
Flexural Strength =
182.8 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Strength
182.8
MPa
26510
psi
ASTM D 790
MRC Polymers MAXNITEâ„¢ 550 GF30 PET, 30% Glass Mineral Reinforced
Information provided by MRC Polymers Inc.