Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 18.8 MPa | 2730 psi | ASTM D790 |
Multibase Multi-Flamâ„¢ 2702 PP Black Polypropylene Features:Halogenated Forms:PelletsInformation provided by Multibase |
|||
Flexural Strength | 18.8 MPa | 2730 psi | ASTM D790 |
BCC Products LIK-WOOD BC 8007 Urethane Casting Lik-Wood is a low viscosity, quick setting, easy to use casting material. A model or tool cast from Lik-Wood will weigh 60% less than other filled urethane systems. Within 30 minutes after mixing an.. |