Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 17.9 MPa | 2600 psi | ASTM D790 |
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet) |
|||
Flexural Strength | 17.9 MPa | 2600 psi | ASTM-F417 |
CoorsTek PolyGlyde™ 1000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |