Polymer Property : Flexural Strength = 16003 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 110.34 MPa
16003 psi
ASTM D790
Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade
Add "R" for Added ReleaseAdd "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.